This Standard Reference Material (SRM ®) is intended primarily for use in evaluating analytical methods and instruments used for the determination of the mass fraction values of selected elements and proximates in marine bivalve tissue, foods, or similar materials. A unit of NIST-1566b contains approximately 25 g of freeze-dried oystertissue. /// Sample value(s) - please ask for current certificate.
Contents
Analyte
CAS Number
Concentration
Unit
Additional information
Method
Calcium (Ca)
[7440-70-2]
0,0838 ± 0,0020
%
Certified value
Chlorine (Cl)
[7782-50-5]
0,514 ± 0,010
%
Certified value
Magnesium (Mg)
[7439-95-4]
0,1085 ± 0,0023
%
Certified value
Potassium (K)
[7440-09-7]
0,652 ± 0,009
%
Certified value
Sodium (Na)
[7440-23-5]
0,3297 ± 0,0053
%
Certified value
Sulfur (S)
[7704-34-9]
0,6887 ± 0,0140
%
Certified value
Aluminium (Al)
[7429-90-5]
197,2 ± 6,0
mg/kg
Certified value
Arsenic (As)
[7440-38-2]
7,65 ± 0,65
mg/kg
Certified value
Cadmium (Cd)
[7440-43-9]
2,48 ± 0,08
mg/kg
Certified value
Cobalt (Co)
[7440-48-4]
0,371 ± 0,009
mg/kg
Certified value
Copper (Cu)
[7440-50-8]
71,6 ± 1,6
mg/kg
Certified value
Iron (Fe)
[7439-89-6]
205,8 ± 6,8
mg/kg
Certified value
Lead (Pb)
[7439-92-1]
0,308 ± 0,009
mg/kg
Certified value
Manganese (Mn)
[7439-96-5]
18,5 ± 0,2
mg/kg
Certified value
Mercury (Hg) total
0,0371 ± 0,0013
mg/kg
Certified value
Methylmercury (as Hg)
0,0132 ± 0,0007
mg/kg
Certified value
Nickel (Ni)
[7440-02-0]
1,04 ± 0,09
mg/kg
Certified value
Rubidium (Rb)
[7440-17-7]
3,26 ± 0,14
mg/kg
Certified value
Selenium (Se)
[7782-49-2]
2,06 ± 0,15
mg/kg
Certified value
Silver (Ag)
[7440-22-4]
0,666 ± 0,009
mg/kg
Certified value
Thorium (Th)
[7440-29-1]
0,0367 ± 0,0043
mg/kg
Certified value
Vanadium (V)
[7440-62-2]
0,577 ± 0,023
mg/kg
Certified value
Zinc (Zn)
[7440-66-6]
1424 ± 46
mg/kg
Certified value
Nitrogen (N)
[7727-37-9]
7,6 ± 0,4
%
Reference value
Antimony (Sb)
[7440-36-0]
0,011 ± 0,002
%
Reference value
Strontium (Sr)
[7440-24-6]
6,8 ± 0,2
%
Reference value
Barium (Ba)
[7440-39-3]
8,6 ± 0,3
%
Reference value
Tin (Sn)
[7440-31-5]
0,031 ± 0,008
%
Reference value
Boron (B)
[7440-42-8]
4,5 ± 1,9
%
Reference value
Titanium (Ti)
[7440-32-6]
12,24 ± 0,39
%
Reference value
Gold (Au)
[7440-57-5]
0,0106 ± 0,0028
%
Reference value
Uranium (U)
[7440-61-1]
0,2550 ± 0,0014
%
Reference value
Hydrogen (H)
[1333-74-0]
7,2 ± 0,4
%
Reference value
Moisture
4,6 ± 3,6
%
Reference value, Mass Fraction as received
Moisture
0 (by definition)
%
Reference value, Mass Fraction dry-mass basis
Solids
95,4 ± 3,6
%
Reference value, Reference value, Mass Fraction as received
View all available product details e.g. description, analytes/parameters, CAS Number, concentrations/values, sales unit/product format, method, source, transport information
NIST provides over 1300 Standard Reference Materials® as well as articles and practice guides describing the development, analysis and use of SRMs.
NIST Standard Reference Materials are used by analytical laboratories in industry, academia and government in order to facilitate commerce and trade and to advance research and development. The SRMs are produced by the engineering laboratory, the material measurement laboratory, and the physical measurement laboratory at NIST. They are available for chemical composition, physical properties, and engineering materials.