Loss of Mass, 110-1000°C as H 2O and C
|
|
k. A. |
18,4 ± 0,2 |
% |
LECO or TGA |
|
Aluminum as Al2O3
|
|
k. A. |
26,9 ± 0,6 |
% |
Alcan SM 1359-99, XRF, glass beads/ICP |
|
Iron as Fe2O3
|
|
k. A. |
4,0 ± 0,4 |
% |
Alcan SM 1359-99, XRF, glass beads/ICP |
|
Silicon as SiO2
|
|
k. A. |
15,7 ± 0,5 |
% |
Alcan SM 1359-99, XRF, glass beads/ICP |
|
Titanium as TiO2
|
|
k. A. |
8,2 ± 0,2 |
% |
Alcan SM 1359-99, XRF, glass beads/ICP |
|
Chromium as Cr2O3
|
|
k. A. |
0,16 ± 0,01 |
% |
Alcan SM 1359-99, XRF, glass beads/ICP |
|
Calcium as CaO
|
|
k. A. |
16,5 ± 0,4 ± Alcan |
% |
SM 1359-99, XRF, glass beads/ICP |
|
Phosphorus as P2O5
|
|
k. A. |
0,21 ± 0,03 |
% |
Alcan SM 1359-99, XRF, glass beads/ICP |
|
Zirconium as ZrO2
|
|
k. A. |
0,28 ± 0,03 |
% |
Alcan SM 1359-99, XRF, glass beads/ICP |
|
Zinc as ZnO
|
|
k. A. |
0,01 ± 0,001 ± Alcan |
% |
SM 1359-99, XRF, glass beads/ICP |
|
Manganese as MnO
|
|
k. A. |
0,013 ± 0,004 |
% |
Alcan SM 1359-99, XRF, glass beads/ICP |
|
Vanadium as V2O5
|
|
k. A. |
0,16 ± 0,03 |
% |
Alcan SM 1359-99, XRF, glass beads/ICP |
|
Potassium as K2O
|
|
k. A. |
0,02 ± 0,01 |
% |
Alcan SM 1359-99, XRF, glass beads/ICP |
|
Magnesium as MgO
|
|
k. A. |
0,03 ± 0,01 |
% |
Alcan SM 1359-99, XRF, glass beads/ICP |
|
Sodium as Na2O
|
|
k. A. |
8,4 ± 0,2 |
% |
Alcan SM 1359-99, XRF, glass beads/ICP |
|
g-Al2O3 as Al2O3
|
|
k. A. |
0,05 ± 0,04 |
% |
DSC Alcan SM 1029-00 |
|
Total Extratable Alumina as Al2O3
|
|
k. A. |
12,2 ± 0,8 |
% |
Alcan SM 1177-04 , high temperature digestion1 |
|
Total Organic Carbon as C
|
|
k. A. |
0,25 ± 0,02 |
% |
Wet Oxidation |
|